Tracking efficiency and charge sharing of 3D silicon sensors at different angles in a 1.4 T magnetic field

H.G Gjersdal, E. B. Bolle, M. B. Borri, C. D. V. Da Via, T. Slavíček

Abstrakt

A 3D silicon sensor fabricated at Stanford with electrodes penetrating throughout the entire silicon wafer and with active edges was tested in a 1.4 T magnetic field with a 180 GeV/c pion beam at the CERN SPS in May 2009. The device under test was bump-bonded to the ATLAS pixel FE-I3 readout electronics chip. Three readout electrodes were used to cover the long pixel side, this resulting in a p-n inter-electrode distance of . Its behavior was confronted with a planar sensor of the type presently installed in the ATLAS inner tracker. Time over threshold, charge sharing and tracking efficiency data were collected at zero and 15° angles with and without magnetic field. The latest is the angular configuration expected for the modules of the Insertable B-Layer (IBL) currently under study for the LHC phase 1 upgrade expected in 2014.

Klíčová slova

Konference

7th International 'Hiroshima' Symposium on the Development and Application of Semiconductor Tracking Detectors Hiroshima, Japan · 2009-08-29